DX52D+Z/+ZM
Specification details for DX52D+Z/+ZM

EN-Product-Metallic coated-Forming-All Grades OverviewTSUK

Overview

Overview

With MagiZinc® you can manufacture lighter products with higher strength thanks to the improved corrosion protection and at the same time increase the production volume and further reduce costs thanks to the better processing properties.
 

Relationship with standards

Metallic coated steel for forming complies with the following European standard

European standardVDA standard
EN 10346: 2015VDA 239-100-16
DX51D+Z/+ZF/+ZM-
DX52D+Z/+ZF/+ZMCR1-GI/GA/ZM
DX53D+Z/+ZF/+ZMCR2-GI/GA/ZM
DX54D+Z/+ZF/+ZMCR3-GI/GA/ZM
DX56D+Z/+ZF/+ZMCR4-GI/GA/ZM
DX57D+Z/+ZMCR5-GI/ZM
DX58D+Z 1-
Galvannealed (ZF/GA) coatings and DX58D+Z are produced in the Netherlands.  For further information click here.
1. Not in standard. Tata Steel’s own specification.

EN-Product-Metallic coated-All Grades Coatings Surface aspectsTSUK

Coatings and surface aspects

Coatings

Three types of metallic coating are available:

Pure zinc

Galvanised steel (Z/GI) is coated with an almost pure zinc coating (>99% zinc).

Zinc-iron alloy

Produced in the Netherlands.  For further information click here.

MagiZinc

MagiZinc steel (ZM) is coated with a zinc coating containing additional magnesium and aluminium.
 

Coating weight

CoatingMinimumMaximum
Pure zinc (Z/GI)90 (6 µm/side)275 (20 µm/side)
MagiZinc (ZM)170 (5 µm/side)310 (22 µm/side)
Coating weight measured in g/m2 double-sided (µm, per side).
 

Surface quality

Surface quality complies with standard: EN 10346:2015. Galvanised steels are available in surface quality A, B or C.
Also, Serica FLO® surface quality produced in the Netherlands.  For further information click here.

Surface quality A: as coated surface

Imperfections such as pimples, marks, scratches, pits, variations in surface appearance, dark spots, stripe marks and light passivation stains are permissible.
Stretch levelling breaks or run-off marks may appear. Coil breaks and stretcher strains may also appear.

Surface quality B: improved surface

With this surface quality, small imperfections such as stretch levelling breaks, skin pass marks, slight scratches, indentations, surface structure, zinc run-off marks and light passivation stains are permissible.

Surface quality C: best quality surface

Surface condition C is obtained by skin passing. The controlled surface for the exposed side enables application of a uniform paint finish. The reverse surface has, at least, the characteristics of surface quality B.
 

Surface finish

Pure zinc

MA: minimised spangle, as coated surface (Z/GI).
MB: minimised spangle, improved surface (Z/GI).
MC: minimised spangle, best quality surface (Z/GI).

MagiZinc®

A : as coated surface (ZM).
B : improved surface (ZM).
C: best quality surface (ZM).

 

Surface roughness

Metallic coated steel (with the exception of galvanised steel with standard surface (MA) can be supplied in various grades of roughness – please contact us for more details. If no roughness is specified, roughness will be as shown in the table below.

Roughness Ra (µm)

 

cut off 0.8mm

cut off 2.5mm

0.6 - 1.90.7 - 2.2

 

Surface treatments

The surface treatments available are O, C and CO.

Oiling (O)

The material surface can be oiled with preservative oil. Other types of oil - for increasing strength or reducing weight – are available to help achieve your optimum performance parameters. Please contact us for details.

Tata Steel offers the following range of oiling levels:

Coating typeCapability
Pure zinc (Z/GI)0.5 - 1.6 g/m2
MagiZinc® (ZM)0.5 - 1.6 g/m2

Other oiling levels are available on request.

Chromium-free passivation (C)

This surface treatment temporarily protects the zinc-coated material against white rust during transportation and storage (not applicable to all qualities and dimensions – please contact us for details).

Chromium-free passivation and oiled (CO)

Please request this combination of surface treatments if you require extra protection against white rust formation (not applicable to all qualities and dimensions – please contact us for details).

T-treatment

Please contact us for further information.

Prime Lubrication Treatment (PLT)

Prime Lubrication Treatment facilitates the manufacturing of stamped components by minimising known issues in stamping and joining.
Currently Under development, please contact us regarding further information

Untreated (U)

Please contact us regarding the availability of untreated coils.

EN-Product-Metallic coated-Forming-DX52D-PropertiesTSUK

Properties

Properties


Mechanical properties

Metallic coated steel for forming has the following mechanical properties. These are measured transverse to the rolling direction:

EN 10346: 2015 Grade DX52D+Z/+ZM
Yield strength 1 Re N/mm² 140 - 300 3
Tensile strength Rm N/mm² 270 - 420
Elongation 2 % 26
Min. r-value   -
Min. n-value   -
1. If the yield point is not pronounced, the values apply to the 0.2% - proof strength Rp0.2 ; if the yield strength is pronounced, the values apply to the lower yield point ReL.
2. Decreased minimum elongation values apply for product thickness t ≤ 0.50 mm (minus 4 units) and for 0.50 mm ≤ t ≤ 0.70 mm (minus 2 units).
Elongation after fracture A uses test piece length L0 = 80 mm.
3. This value applies to skin-passed products only (surface qualities B and C).
 

Chemical composition

Tata Steel complies with the following cast analysis:

EN 10346: 2015 Grade DX52D+Z/+ZM
C Max. 0.12
Mn Max. 0.60
P Max. 0.10
S Max. 0.045
Si Max. 0.50
Al Min. -
N Max. -
Ti Max. 0.30
All values are in weight%.

EN-Product-Metallic coated-Forming-DX52D-Dimensions TSUK

Dimensions

Dimensional capability
 

Galvanised (Z/GI) products

Dimensions in mm.

ThicknessMax. width
From - up toDX52D
0.40 - 0.551375
0.55 - 0.601525
0.60 - 0.651575
0.65 - 0.661640
0.66 - 1.251650
1.25 - 1.651640
1.65 - 2.001380
For widths below 900 mm, please contact us.
For products produced in the Netherlands click here.

Galvannealed (ZF) products

Produced in the Netherlands.  For further information click here.

MagiZinc® (ZM) products

Dimensions in mm.

ThicknessMax. width
From - up toDX52D
0.60 - 0.651575
0.65 - 0.661640
0.66 - 1.251650
1.25 - 1.651640
1.65 - 1.801380
1.80 - 2.001380
For widths below 900 mm, please contact us.
For thicknesses between 2.00 and 2.50 mm, please contact us.
For products produced in the Netherlands click here.

Tolerances

Tolerances comply with standard EN 10143 2006.
Tighter tolerances are available, please contact us for details.

EN-Product-Metallic Coated-All Grades Shape and Dimensional TolerancesTSUK

Shape and dimensional tolerances

Tolerances on thickness

The tolerances comply with standard EN 10143: 2006.
Tighter tolerances are available on request.
Thickness tolerance availability is shown below:

Thickness tolerance

Availability

Full thickness tolerance

Available

Special thickness tolerance

Available

50% of full thickness tolerance

Refer before ordering

 

The following tolerances apply to the grades with a minimum value for the yield strength lower than 260N/mm².

Nominal
thickness

Normal tolerances for a nominal width of 1 2

Special tolerances (S) for a
nominal width of 1 2

 

≤ 1200

> 1200

> 1500

≤ 1200

> 1200

> 1500

 

≤ 1500

 

 

≤ 1500

 

> 0.40

≤ 0.60

± 0.04

± 0.05

± 0.06

± 0.035

± 0.040

± 0.045

> 0.60

≤ 0.80

± 0.05

± 0.06

± 0.07

± 0.040

± 0.045

± 0.050

> 0.80

≤ 1.00

± 0.06

± 0.07

± 0.08

± 0.045

± 0.050

± 0.060

> 1.00

≤ 1.20

± 0.07

± 0.08

± 0.09

± 0.050

± 0.060

± 0.070

> 1.20

≤ 1.60

± 0.10

± 0.11

± 0.12

± 0.060

± 0.070

± 0.080

> 1.60

≤ 2.00

± 0.12

± 0.13

± 0.14

± 0.070

± 0.080

± 0.090

> 2.00

≤ 2.50

± 0.14

± 0.15

± 0.16

± 0.090

± 0.100

± 0.110

> 2.50

≤ 3.00

± 0.17

± 0.17

± 0.18

± 0.110

± 0.120

± 0.130

> 3.00

≤ 5.00

± 0.20

± 0.20

± 0.21

± 0.15

± 0.16

± 0.17

> 5.00

≤ 6.50

± 0.22

± 0.22

± 0.23

± 0.17

± 0.18

± 0.19

1. Around cold-rolled welds an increase of 20% at the most over the thickness tolerance is allowed
   over a length of 15 metres.
2. For zinc coatings ≥ Z450 the tolerance on the thickness must be raised by 0.02mm.
The following tolerances apply to the steel grades with a minimum value for the yield strength 260N/mm² ≤ Rp0.2 < 360N/mm² and for grades DX51D and S550GD.

Nominal
thickness

Normal tolerances for a nominal width of 1 2

Special tolerances (S) for a
nominal width of 1 2

 

≤ 1200

> 1200

> 1500

≤ 1200

> 1200

> 1500

 

≤ 1500

 

 

≤ 1500

 

≥ 0.35

≤ 0.40

± 0.05

± 0.06

-

± 0.035

± 0.040

-

> 0.40

≤ 0.60

± 0.05

± 0.06

± 0.07

± 0.040

± 0.045

± 0.050

> 0.60

≤ 0.80

± 0.06

± 0.07

± 0.08

± 0.045

± 0.050

± 0.060

> 0.80

≤ 1.00

± 0.07

± 0.08

± 0.09

± 0.050

± 0.060

± 0.070

> 1.00

≤ 1.20

± 0.08

± 0.09

± 0.11

± 0.060

± 0.070

± 0.080

> 1.20

≤ 1.60

± 0.11

± 0.13

± 0.14

± 0.070

± 0.080

± 0.090

> 1.60

≤ 2.00

± 0.14

± 0.15

± 0.16

± 0.080

± 0.090

± 0.110

> 2.00

≤ 2.50

± 0.16

± 0.17

± 0.18

± 0.110

± 0.120

± 0.130

> 2.50

≤ 3.00

± 0.19

± 0.20

± 0.20

± 0.130

± 0.140

± 0.150

> 3.00

≤ 5.00

± 0.22

± 0.24

± 0.25

± 0.17

± 0.18

± 0.19

> 5.00

≤ 6.50

± 0.24

± 0.25

± 0.26

± 0.19

± 0.20

± 0.21

1. Around cold-rolled welds an increase of 20% at the most over the thickness tolerance is allowed
   over a length of 15 metres.
2. For zinc coatings ≥ Z450 the tolerance on the thickness must be raised by 0.02mm
The following tolerances apply to the steel grades with a minimum value for the yield strength 360N/mm² ≤ Rp0.2 ≤ 420N/mm².

Nominal
thickness

Normal tolerances for a nominal width of 1 2

Special tolerances (S) for a
nominal width of 1 2

 

≤ 1200

> 1200

> 1500

≤ 1200

> 1200

> 1500

 

≤ 1500

 

 

≤ 1500

 

≥ 0.35

≤ 0.40

± 0.05

± 0.06

-

± 0.040

± 0.045

-

> 0.40

≤ 0.60

± 0.06

± 0.07

± 0.08

± 0.045

± 0.050

± 0.060

> 0.60

≤ 0.80

± 0.07

± 0.08

± 0.09

± 0.050

± 0.060

± 0.070

> 0.80

≤ 1.00

± 0.08

± 0.09

± 0.11

± 0.060

± 0.070

± 0.080

> 1.00

≤ 1.20

± 0.10

± 0.11

± 0.12

± 0.070

± 0.080

± 0.090

> 1.20

≤ 1.60

± 0.13

± 0.14

± 0.16

± 0.080

± 0.090

± 0.110

> 1.60

≤ 2.00

± 0.16

± 0.17

± 0.19

± 0.090

± 0.110

± 0.120

> 2.00

≤ 2.50

± 0.18

± 0.20

± 0.21

± 0.120

± 0.130

± 0.140

> 2.50

≤ 3.00

± 0.22

± 0.22

± 0.23

± 0.140

± 0.150

± 0.160

> 3.00

≤ 5.00

± 0.22

± 0.24

± 0.25

± 0.17

± 0.18

± 0.19

> 5.00

≤ 6.50

± 0.24

± 0.25

± 0.26

± 0.19

± 0.20

± 0.21

1. Around cold-rolled welds an increase of 20% at the most over the thickness tolerance is allowed
   over a length of 15 metres.
2. For zinc coatings ≥ Z450 the tolerance on the thickness must be raised by 0.02mm.
The following tolerances apply to the steel grades with a minimum value for the yield strength 420N/mm² < Rp0.2 ≤ 900N/mm².

Nominal
thickness

Normal tolerances for a nominal width of 1 2

Special tolerances (S) for a
nominal width of 1 2

 

≤ 1200

> 1200

> 1500

≤ 1200

> 1200

> 1500

 

≤ 1500

 

 

≤ 1500

 

≥ 0.35

≤ 0.40

± 0.06

± 0.07

-

± 0.045

± 0.050

-

> 0.40

≤ 0.60

± 0.06

± 0.08

± 0.09

± 0.050

± 0.060

± 0.070

> 0.60

≤ 0.80

± 0.07

± 0.09

± 0.11

± 0.060

± 0.070

± 0.080

> 0.80

≤ 1.00

± 0.09

± 0.11

± 0.12

± 0.070

± 0.080

± 0.090

> 1.00

≤ 1.20

± 0.11

± 0.13

± 0.14

± 0.080

± 0.090

± 0.110

> 1.20

≤ 1.60

± 0.15

± 0.16

± 0.18

± 0.090

± 0.110

± 0.120

> 1.60

≤ 2.00

± 0.18

± 0.19

± 0.21

± 0.110

± 0.120

± 0.140

> 2.00

≤ 2.50

± 0.21

± 0.22

± 0.24

± 0.140

± 0.150

± 0.170

> 2.50

≤ 3.00

± 0.24

± 0.25

± 0.26

± 0.170

± 0.180

± 0.190

> 3.00

≤ 5.00

± 0.26

± 0.27

± 0.28

± 0.23

± 0.24

± 0.26

> 5.00

≤ 6.50

± 0.28

± 0.29

± 0.30

± 0.25

± 0.26

± 0.28

1. Around cold-rolled welds an increase of 20% at the most over the thickness tolerance is allowed
   over a length of 15 metres.
2. For zinc coatings ≥ Z450 the tolerance on the thickness must be raised by 0.02mm.

 

Tolerances on width

The tolerances on width comply with standard EN 10143: 2006
MagiZinc is not included in the standard, but fulfils EN 10143: 2006 requirements.
Tighter tolerances are available on request.

Tolerances in mm.

Nominal width w Normal tolerances Special tolerances (S)
600 ≤ w ≤ 1200 + 5
0
+ 2
0
1200 < w ≤ 1500 + 6
0
+ 2
0
1500 < w ≤ 1800 + 7
0
+ 3
0
w > 1800 + 8
0
+ 3
0

 

Dimensions and coil weights

Description Availability
Coil diameter inner 610mm
(508 mm available on request)
Coil diameter outer 10/7 x width max
1000mm min.
2500mm max.
Coil weight 30t max.
Coil weight limited by maximum outer diameter
Maximum weight allowed by road/rail transport
Some products may have different coil weight ranges available
Usually a minimum coil weight up to 85% of the maximum coil weight can be requested
Minimum tonnage per order Refer to price list for order quantity details
Minimum order quantities may apply

 

EN-Product-Metallic coated-All grades Further processingTSUK

Further processing

Further processing

We have a broad network of Tata Steel service centres across Europe, offering decoiling and slitting services from stock and against short lead times

Light gauge processing

Processing type Slitting Decoiling Blanking
Thickness range (mm) 0.2 - 7.0 0.3 - 6.0 0.3 - 6.0
Width range (mm) 10 - 2050 50 - 2600 200 - 2600
Length range - up to 6m up to 6m
Locations UK
Ireland
Netherlands
Germany
France
Spain
Sweden
Norway
Finland
UK
Ireland
Netherlands
Germany
France
Spain
Sweden
Norway
Finland
UK
Netherlands

For further information please visit our Service Centre webpages.