Advanced and ultra high-strength steel (AHSS / UHSS)
Tata Steel’s range of versatile hot-rolled advanced and ultra high-strength steels has been developed primarily to meet the needs of the automotive industry – increasing strength or reducing weight to help achieve optimal performance parameters.
EN_US-Product-Hot-Rolled-AHSS-HR FB590-UC TSUK
EN_US-Product-Hot-Rolled-AHSS UHSS-All grades overview TSUK
Ferrite-bainite – HR FB590-UC
HR FB590-UC is a ferrite-bainite advanced high-strength steel offering excellent formability characteristics. It is particularly suited to automotive chassis and suspension applications where a combination of superior strength and fatigue performance is required on relatively complex-shaped parts. HR FB590-UC offers a high hole expansion capacity (HEC) and high tensile strength – ideal for components with a significant amount of edge stretching. The tensile strength levels deliver excellent fatigue resistance as an additional benefit.
Relationship with standards
Tata Steel can supply the following hot-rolled advanced and ultra high-strength steel grades:
Tata Steel | VDA | prEN 10338:2009 | EN 10083-3:2006 |
---|---|---|---|
HR FB590-UC | HR440Y580T-FB | HDT580F | - |
HR XPF800-UC* | - | - | - |
HR XPF1000-UC* | - | - | - |
HR CP800-UC* | HR660Y760T-CP | HDT760C | - |
*Produced in the Netherlands. For further information click here.
Applications
- upper and lower control arms
- engine sub-frames
- other chassis and suspension components
- twist beam rear axles
- wheels
Strength and ductility
Utilising the superior combination of strength and ductility of Tata Steel’s advanced steel portfolio can yield significant lightweighting potential. Component shapes which were previously considered too challenging to make, are now a possibility. This enables designers to integrate high strength and durable materials into their designs to fully unlock the potential of steel.
Increased performance
Application of our advanced steel grades – in place of lower strength, conventional steel grades - can lead to the increased performance of finished components.
Weight reduction
Application of our advanced steel with a lower thickness - in comparison with lower strength, conventional steel grades - can help reduce component weight without compromising performance. This can increase your output per tonne of steel.
Product choice
Our hot-rolled advanced and ultra high-strength steels include ferrite-bainite, complex phase and hot forming steel grades.
Supply - product conditions
Hot-rolled steel can be supplied with these product conditions and finishes and with this surface treatment:
Side/surface condition | non-pickled | pickled | pickled and oiled |
---|---|---|---|
Mill edges | Yes | Yes | Yes |
Trimmed edges | - | Yes | Yes |
Trimmed edges available in thicknesses up to 5.0 mm.
Please contact us regarding other specifications we may have that meet your needs.
Surface aspects
Description | Availability |
---|---|
Surface finish | Coils are available in non-pickled and pickled finish for most grades. For grade specific availability, please refer to the dimensional tables. |
Oiling | Pickled finish is available with rolling or preservative oil applied. Oil weight normally 0.4-1.8 g/m2 |
Alternative oiling ranges are available.
Please contact us for details.
Certification
Test certificates 2.2/3.1 are available according to EN 10204.
EN_US-Product-Hot-rolled-All Grades Surface aspects Supply Conditions TSUK
Hot-rolled steel can be supplied with these product conditions and finishes and with this surface treatment:
Side/surface condition | non-pickled | pickled | pickled and oiled |
---|---|---|---|
Mill edges | Yes | Yes | Yes |
Trimmed edges | - | Yes | Yes |
Trimmed edges available in thicknesses up to 0.25 inch.
The steel grades shown on the following pages belong to the standard range offered by Tata Steel.
Please contact us regarding other specifications we may have that meet your needs. You can find details on how to get in touch with us in 'Contact Us' below.
Surface aspects
Description | Availability |
---|---|
Surface finish | Coils are available in non-pickled and pickled finish for most grades. For grade specific availability, please refer to the dimensional tables. |
Oiling | Pickled finish is available with rolling or preservative oil applied. Oil weight normally 55 - 275 mg/ft2 |
Alternative oiling ranges are available.
Please contact us for details. You can find details on how to get in touch with us in 'Contact Us' below.
EN_US-Product-Hot-Rolled-AHSS-FB590-Properties TSUK
Mechanical Properties
The values shown for the mechanical properties of HR FB590 are for test pieces taken parallel to the rolling direction unless otherwise stated.
EN 10338: HDT580F | FB590 HR Typical2 | |||
---|---|---|---|---|
Yield strength Rp0,2 1 (N/mm²) | 440 - 600 | 490 | 480-600 | |
Tensile strength Rm (N/mm²) | ≥ 580 | 595 | 590-670 | |
Elongation % | > 15 | 20 | 18 |
1. Lower yield strength or 0.2 % proof stress applies.
2. These mechanical property values are quoted for the transverse rolling direction.
Hole expansion coefficient values can be supplied (although not as part of the production release test) – please contact us for details.
Elongation after fracture A uses test piece length L0 = 80 mm
Chemical composition
Tata Steel supplies the following cast analysis with maximum values in weight percentages unless shown otherwise:
EN10338: HDT580F | FB590 HR | ||
---|---|---|---|
C | Max. | 0.18 | 0.12 |
Mn | Max. | 2.0 | 2.0 |
Si | Max. | 0.5 | |
P | Max. | 0.05 | 0.025 |
S | Max. | 0.010 | 0.010 |
Altot | 0.015 - 2.0 | 0.015 - 2.0 | |
Cr+Mo | Max. | 1.0 | 1.0 |
Nb | Max. | 0.09 | |
Ti | Max. | 0.15 | |
Nb+Ti | Max. | 0.15 | |
CrMoCu | Max. | 1.0 | |
TiNbV | Max. | 0.15 | |
V | Max. | 0.15 | 0.15 |
B | Max. | 0.01 | 0.01 |
EN_US-Product-Hot-Rolled-AHSS-FB590-Dimensions TSUK
Dimensions
HR FB590 is available in pickled and non-pickled condition.
Dimensions in mm.
Thickness | Max. width |
---|---|
From - to | HR FB590 |
2.00 - 2.50 | 1100 |
2.50 - 2.80 | 1300 |
2.80 - 5.00 | 1360 |
Minimum width is 900 mm.
For products produced in the Netherlands click here.
Tolerances for wide strip and slit wide strip comply with standard EN 10051: 2010.
Tighter tolerances are available, please contact us.
EN_US-Product-Hot-rolled-All grades Shape and dimensional tolerancesTSUK
Shape and dimensional tolerances
Tolerances on thickness
Tata Steel can supply to full thickness tolerance specified in ASTM A568: 2015 / A635: 2015.
Thickness tolerances over, no tolerance under.
Tighter tolerances are available as shown below:
Carbon Steel | Thickness tolerances available | ||||
---|---|---|---|---|---|
ASTM A 568 (2015) / A635 (2015) | |||||
20 - 40 | 40 - 48 | 48 - 60 | 60 - 72 | >72 | |
0.031 - 0.051 | 0.01 | 0.01 | 0.01 | 0.01 | 0.01 |
0.051 - 0.057 | 0.01 | 0.012 | 0.012 | 0.014 | 0.014 |
0.057 - 0.071 | 0.012 | 0.012 | 0.014 | 0.014 | 0.014 |
0.071 - 0.098 | 0.014 | 0.014 | 0.014 | 0.016 | 0.016 |
0.098 - 0.179 | 0.014 | 0.016 | 0.016 | 0.016 | 0.016 |
0.179 - 0.229 | 0.016 | 0.018 | 0.02 | 0.022 | 0.024 |
0.229 - 0.313 | 0.022 | 0.024 | 0.024 | 0.026 | 0.03 |
0.313 - 0.375 | 0.024 | 0.026 | 0.028 | 0.03 | 0.032 |
0.375 - 0.500 | 0.028 | 0.028 | 0.03 | 0.032 | 0.036 |
0.500 - 0.625 | 0.03 | 0.03 | 0.032 | 0.036 | 0.038 |
0.625 - 1.000 | 0.032 | 0.032 | 0.034 | 0.038 | 0.04 |
HSLA | Thickness tolerances available | ||||||
---|---|---|---|---|---|---|---|
ASTM A568 (2015) / A635 (2015) | |||||||
20 - 32 | 32 - 40 | 40 - 48 | 48 - 60 | 60 - 72 | 72 - 80 | > 80 | |
0.031 - 0.051 | 0.012 | 0.012 | 0.012 | 0.012 | 0.012 | 0.012 | 0.012 |
0.051 - 0.059 | 0.012 | 0.012 | 0.014 | 0.014 | 0.014 | 0.014 | 0.014 |
0.059 - 0.070 | 0.014 | 0.014 | 0.014 | 0.014 | 0.016 | 0.016 | 0.016 |
0.070 - 0.082 | 0.014 | 0.014 | 0.014 | 0.014 | 0.016 | 0.016 | 0.016 |
0.082 - 0.098 | 0.014 | 0.016 | 0.116 | 0.016 | 0.018 | 0.018 | 0.02 |
0.098 - 0.179 | 0.016 | 0.016 | 0.02 | 0.02 | 0.022 | 0.024 | 0.024 |
0.179 - 0.229 | 0.018 | 0.018 | 0.02 | 0.02 | 0.022 | 0.024 | 0.024 |
0.229 - 0.313 | 0.022 | 0.022 | 0.024 | 0.024 | 0.026 | 0.03 | 0.03 |
0.313 - 0.375 | 0.024 | 0.024 | 0.026 | 0.028 | 0.03 | 0.032 | 0.032 |
0.375 - 0.500 | 0.028 | 0.028 | 0.028 | 0.03 | 0.032 | 0.036 | 0.036 |
0.500 - 0.625 | 0.03 | 0.03 | 0.03 | 0.032 | 0.036 | 0.038 | 0.038 |
0.625 - 1.000 | 0.032 | 0.032 | 0.032 | 0.034 | 0.038 | 0.04 | 0.04 |
Option for maximum crown values
At the time of ordering, specific agreements can be made on the crown of hot-rolled strip.
Tolerances on width, edge camber and flatness
Material will be supplied conforming to the tolerances specified in ASTM A568 (2015) / A635 (2015). Width tolerances are over, no tolerance under.
Width tolerances available | ||
---|---|---|
Carbon steel | ASTM A568: 2015 / A635: 2015 | |
Mill edge | Cut edge | |
24 - 26 | 0.812 | 0.125 |
26 - 28 | 0.937 | 0.125 |
28 - 30 | 0.937 | 0.125 |
30 - 35 | 1.125 | 0.187 |
35 - 48 | 1.125 | 0.187 |
48 - 50 | 1.125 | 0.25 |
50 - 60 | 1.5 | 0.25 |
60 - 65 | 1.5 | 0.312 |
65 - 70 | 1.5 | 0.312 |
70 - 78 | 1.5 | 0.312 |
78 - 80 | 1.875 | 0.312 |
80 - 82 | 1.875 | 0.375 |
Width tolerances available | ||
---|---|---|
HSLA | ASTM A568: 2015 / A635: 2015 | |
Mill edge | Cut edge | |
24 - 26 | 0.812 | 0.125 |
26 - 28 | 0.937 | 0.125 |
28 - 30 | 1.125 | 0.125 |
30 - 35 | 1.125 | 0.187 |
35 - 48 | 1.25 | 0.187 |
48 - 50 | 1.25 | 0.25 |
50 - 60 | 1.5 | 0.25 |
60 - 65 | 1.625 | 0.312 |
65 - 70 | 1.75 | 0.312 |
70 - 78 | 1.875 | 0.312 |
78 - 80 | 2 | 0.375 |
80 - 82 | 1.875 | 0.375 |
Dimensions and coil weights
Tata Steel can supply hot-rolled steels with the following minimum and maximum dimensions and weights.
Description | Capability |
---|---|
Coil diameter inner non-pickled | 30 inch |
Coil diameter inner pickled | 24 inch standard |
30 inch on request | |
Tolerance on inner diameter | +0/-2 inch |
Coil diameter outer non-pickled | Outer diameter available is 10/7 x width to reduce possibility of coil tipping over |
Max. 86 inch | |
Min. 41.5 inch | |
Coil diameter outer pickled and oiled | Outer diameter available is 10/7 x width to reduce possibility of coil tipping over |
Max. 86 inch | |
Min. 65 inch | |
Coil weight | Max. 75,000 lbs |
Maximum coil weight limits can vary due to | |
transport limits and outer coil diameter | |
Some HR products may have different coil weight ranges | |
Minimum tonnage per order | Refer to price list for order quantity details |
Minimum order quantities may apply |
EN_US-Product-Hot-Rolled-AHSS UHSS-Downloads TSUK
Download:
EN_US-Tata Steel in the USA and Canada
Tata Steel in the USA and Canada
Chicago office
475 N. Martingale Road, Suite 330
Schaumburg, IL 60173